Nome |
# |
Comparison on mechanical behavior and microstructural features between traditional and AM AISI 316L, file 55dcff89-ba9b-428d-b170-d554f9b930f7
|
40
|
Analysis of fracture characteristics in aluminium-CFRP hybrid laminate subject to three-point bending loading, file 804d0c20-27e7-46fc-9a04-ccf9dc66640e
|
36
|
Impact of Copper, Tin and Titanium Addition on Bending-Induced Damage of Intermetallic Phases in Hot Dip Galvanizing, file d4b50aec-8734-42b8-a988-5ae2fce7b7f9
|
29
|
Effect of recycling on internal and external defects of Ti-6Al-4V powder particles for electron beam melting process, file 659683cd-25b6-42cf-aaaa-cca94056e9f4
|
23
|
Numerical model development to predict the process-induced residual stresses in fibre metal laminates, file 115c1589-36cc-4a32-a0b5-372c36258bc4
|
21
|
Analysis of CFRP/Al hybrid laminates flexural strength, file de2a6153-fef6-86a2-e053-1705fe0a3017
|
21
|
Numerical Modelling of Fibre Metal Laminate Flexural Behaviour, file 0ece9c23-3566-4ae7-95c7-78b1b2f8e1f5
|
20
|
Experimental analysis of aluminium/carbon epoxy hybrid laminates under flexural load, file e2e7224a-9c4c-4e37-9c0c-0713225be24d
|
18
|
Bath chemical composition influence on intermetallic phases damage in hot dip galvanizing, file 0d2ebfb8-0180-4279-b3e0-e5852cd5e15e
|
16
|
Study of the fracture behavior of a CuCrZr alloy, file 9e216e6b-3be2-42ae-ae8b-cc21654a772f
|
16
|
Fracture micrographic analysis of a carbon FML under three-point bending load, file c16f7123-d47f-42b9-8933-6da513917d11
|
15
|
Analysis of acoustic emission entropy for damage assessment of pearlitic ductile cast irons, file de2a6154-4dbf-86a2-e053-1705fe0a3017
|
15
|
Hybrid structures in Titanium-Lattice/FRP: effect of skins material on bending characteristics, file e2aeecb6-d7f1-4c1f-92d5-4b5ecc589a7f
|
15
|
Combination of discrete and finite element method to simulate damage in galvanised steel, file 16a2389b-78c9-4d12-87bf-ebefbc35c36d
|
14
|
Crack micromechanisms in cycled shape memory alloys, file bee3f6d3-a840-45d5-a7f9-9b8dbaad3efd
|
14
|
Flexural strength of aluminium carbon/epoxy fibre metal laminates, file a828749d-ed0c-481d-9c00-caec92a85a18
|
13
|
Damage micromechanisms in ferritic-pearlitic ductile cast irons, file de2a6152-fe1e-86a2-e053-1705fe0a3017
|
9
|
Ductile Damage Evolution Under Different Strain Rate Conditions, file de2a6152-f5ec-86a2-e053-1705fe0a3017
|
7
|
Procedia Structural integrity, file de2a6153-48f2-86a2-e053-1705fe0a3017
|
7
|
Static strength and design of aluminium-to-steel thin welded joints, file de2a6153-feed-86a2-e053-1705fe0a3017
|
6
|
An Innovative Method to Analyse the Geometrical Accuracy of Ti6Al4V Octet-Truss Lattice Structures, file 92390f89-2371-4955-84b4-22b540214ede
|
5
|
Manufacturing process effect on the bending characteristics of titanium-lattice/FRP hybrid structures, file e12bddb9-ed77-4174-a0fe-dc22976d790a
|
5
|
Duplex stainless steels “475°C embrittlement”: influence of the chemical composition on the fatigue crack propagation, file de2a6153-ad2f-86a2-e053-1705fe0a3017
|
4
|
Fatigue crack propagation and damaging micromechanisms in Ductile Cast Irons, file de2a6153-d4df-86a2-e053-1705fe0a3017
|
4
|
Effect of recycling powder on the fatigue properties of AM Ti6Al4V, file 7b205eea-2c96-47d5-8182-5d7405760270
|
3
|
Damaging micromechanisms characterization of a ferritic ductile cast iron, file de2a6152-fe7c-86a2-e053-1705fe0a3017
|
3
|
Graphite nodules and fatigue crack propagation micromechanisms in a ferritic ductile cast iron, file de2a6153-081f-86a2-e053-1705fe0a3017
|
3
|
Mechanical behavior of cycled shape memory alloy, file 39c7513c-68fb-48b6-b3f9-449e5e93b456
|
2
|
Analysis of Hydrothermal Ageing on Mechanical Performances of Fibre Metal Laminates, file 5bba9d1b-249e-41f5-97dc-0aeb59178c5d
|
2
|
Geometrical Accuracy Analysis of Ti-6Al-4V Trusses Manufactured by Electron Beam Melting Process, file 8ea2d647-3661-4d7a-95e9-772aaca69cb4
|
2
|
Mechanical properties gradient in graphite nodules: influence on ferritic DCI damaging micromechanisms, file de2a6153-081c-86a2-e053-1705fe0a3017
|
2
|
Influence of the graphite elements morphology on the fatigue crack propagation mechanisms in a ferritic ductile cast iron, file de2a6153-4be9-86a2-e053-1705fe0a3017
|
2
|
Frattura ed Integrità Strutturale, file de2a6153-4bef-86a2-e053-1705fe0a3017
|
2
|
Grain size and loading conditions influence on fatigue crack propagation in a Cu-Zn-Al shape memory alloy, file de2a6153-de04-86a2-e053-1705fe0a3017
|
2
|
Chemical composition and heat treatment influence on duplex stainless steels fatigue crack propagation resistance, file de2a6153-e1db-86a2-e053-1705fe0a3017
|
2
|
Overload effects on fatigue cracks in a ferritized ductile cast iron, file de2a6153-f6ec-86a2-e053-1705fe0a3017
|
2
|
Performance evaluation of CFRP/Al fibre metal laminates with different structural characteristics, file de2a6153-feee-86a2-e053-1705fe0a3017
|
2
|
Failure energy and strength of Al/CFRP hybrid laminates under flexural load, file 44ae3efb-83f3-44ad-afda-65f5dc12600c
|
1
|
Ferritic and austenitic sintered stainless steels fatigue crack propagation resistance: hydrogen embrittlement resistance, file de2a6152-f5f4-86a2-e053-1705fe0a3017
|
1
|
QUANTITATIVE SHAPE EVALUATION OF GRAPHITE PARTICLES IN DUCTILE IRON, file de2a6152-f777-86a2-e053-1705fe0a3017
|
1
|
Sintered stainless steels: fatigue crack propagation resistance under hydrogen charging conditions, file de2a6152-f942-86a2-e053-1705fe0a3017
|
1
|
Graphite nodule morphology evolution as an indicator of DCI macroscopic damage level, file de2a6153-0818-86a2-e053-1705fe0a3017
|
1
|
Crack path in a Zn-Cu-Al PE alloy under uniaxial load, file de2a6153-081d-86a2-e053-1705fe0a3017
|
1
|
Editorial, file de2a6153-2ae1-86a2-e053-1705fe0a3017
|
1
|
Fatigue crack tip damaging micromechanisms in a ferritic-pearlitic ductile cast iron, file de2a6153-2bc3-86a2-e053-1705fe0a3017
|
1
|
Kinetics of Intermetallic Phases and Mechanical Behavior of ZnSn3% Hot-Dip Galvanization Coatings, file de2a6153-7aa5-86a2-e053-1705fe0a3017
|
1
|
Integranular corrosion susceptibility analysis in austeno-ferritic (duplex) stainless steels, file de2a6153-b804-86a2-e053-1705fe0a3017
|
1
|
Grain size influence on fatigue behaviour in a CuZnAl PE SMA, file de2a6153-e1dd-86a2-e053-1705fe0a3017
|
1
|
Editorial, file de2a6153-f5c6-86a2-e053-1705fe0a3017
|
1
|
Influence of structural characteristics on the interlaminar shear strength of CFRP/Al fibre metal laminates, file de2a6153-f6ef-86a2-e053-1705fe0a3017
|
1
|
Guest editorial: special issue - IGF international - structural integrity, file de2a6153-feeb-86a2-e053-1705fe0a3017
|
1
|
Performance index of isogrid structures: robotic filament winding carbon fiber reinforced polymer vs. titanium alloy, file de2a6154-4a99-86a2-e053-1705fe0a3017
|
1
|
Totale |
417 |